What Is the Difference Between Swiss-Type and Standard CNC Turning?

1 views

Swiss-type CNC uses guide bushings to support bar stock near the tool, enabling the machining of slender parts without deflection. Standard CNC turning employs chucks or collets to hold the workpiece, making it more suitable for shorter parts with larger diameters.

Back to FAQ Center

Related Questions

Related to What Is the Difference Between Swiss-Type and Standard CNC Turning?

Swiss-type CNC easily achieves 20:1 length-to-diameter ratios, surpassing the 10:1 limit of standard turning. With proper tooling and support, some applications can even exceed 50:1.

Read full answer

Yes, modern Swiss-type CNC machines are equipped with multiple tool stations and live tooling capabilities. Off-center operations such as transverse drilling, milling, slotting, and hex broaching can all be completed in a single cycle.

Read full answer

Standard machined surface roughness is 125 Ra (3.2 µm); finish machining achieves 63 Ra (1.6 µm). Post-processing such as sandblasting or polishing can further improve surface quality.

Read full answer

We accept STEP(.stp), IGES(.igs), SolidWorks(.sldprt), Parasolid(.x_t), and STL files. For the most accurate quotes, STEP is the preferred format.

Read full answer

In CNC turning, the workpiece rotates while the tool remains stationary, suitable for cylindrical parts such as shafts, pins, and sleeves. In CNC machining, the workpiece is stationary while the tool rotates, ideal for flat, prismatic and complex 3D geometric shapes.

Read full answer

Send Us Your Drawing — We Handle the Rest

Send your STEP / DWG / PDF drawing and get a detailed quote with free DFM analysis and process recommendations within 2 hours. No minimum order — from 1 piece.

Live inquiries
Michael · GermanyNeed 500 aluminum brackets, please quote
Sophie · FranceLead time for CNC turned stainless shafts?
David · USANeed 1000 injection molded ABS housings
Emma · UKCan you machine 5-axis titanium parts?