Anodizing is primarily used for aluminum alloys (6061, 7075, 2024). Titanium alloys can also be anodized. Other metals such as steel and brass require different surface treatments like electroplating or passivation.
Anodizing is primarily used for aluminum alloys (6061, 7075, 2024). Titanium alloys can also be anodized. Other metals such as steel and brass require different surface treatments like electroplating or passivation.
Related to Which Materials Can Be Anodized?
Type II is standard anodizing with a thinner oxide layer (0.5-1.5 mil), suitable for decoration and corrosion resistance. Type III (hard) anodizing features a thicker oxide layer (1-2 mil) with significantly higher hardness and wear resistance, ideal for functional applications.
Standard machined surface roughness is 125 Ra (3.2 µm); finish machining achieves 63 Ra (1.6 µm). Post-processing such as sandblasting or polishing can further improve surface quality.
We accept STEP(.stp), IGES(.igs), SolidWorks(.sldprt), Parasolid(.x_t), and STL files. For the most accurate quotes, STEP is the preferred format.
Yes, most surface treatments increase the part's surface thickness. Anodization typically adds 0.5-2 mils per side, while electroplating adds 0.1-2 mils depending on the type. Our engineers account for this material allowance during machining to ensure the final dimensions meet specifications.
In CNC turning, the workpiece rotates while the tool remains stationary, suitable for cylindrical parts such as shafts, pins, and sleeves. In CNC machining, the workpiece is stationary while the tool rotates, ideal for flat, prismatic and complex 3D geometric shapes.
Related to Which Materials Can Be Anodized?
Compare aluminum, stainless steel, and titanium for CNC machining. Analyze strength, weight, cost
Compare 6061 vs. 7075 aluminum for CNC machining, covering strength, cutting parameters, and finishes to balance cost and efficiency for precision par…
Based on experience with 72 CNC machines, we analyze root causes of aluminum tolerance issues. Covers material selection and DFA for precise control.
Related to Which Materials Can Be Anodized?
In-depth guide to CNC machining covering 3/5-axis milling and turning. Optimized for engineers and buyers to enhance precision and efficiency.
Learn how Ra values define aluminum surface finish. This guide links roughness metrics to CNC machining capabilities and inspection standards to preve…
By engaging DFM early and optimizing material selection, engineers can reduce machining time, scrap rates
Related to Which Materials Can Be Anodized?
Learn how CNC tolerances impact aluminum part quality and cost. Explore ISO 2768, GD&T, and surface finish.
Based on 72 CNC machines, here are 10 design rules for aluminum precision. Cover wall thickness, tolerance, and DFM to prevent scrap, ensure ±0.01mm a…
Expert CNC aluminum DFM guide: ISO 261 drill formulas, blind hole depth, & thread tolerances for reliable, aerospace-grade assemblies.
Send your STEP / DWG / PDF drawing and get a detailed quote with free DFM analysis and process recommendations within 2 hours. No minimum order — from 1 piece.