Not Just Precision Parts, But Works of Art | Free DFM Analysis & Instant Quotes
Get Instant Quote
Company
Strength
20 Years of Experience
20 Years of Experience
72 Sets of CNC Machines
72 Sets of CNC Machines
Precision: ±0.01mm
Precision: ±0.01mm
7-15 Days Fast Shipping
7-15 Days Fast Shipping
Quality
Advantages
No Knife Marks
No Knife Marks
No Scratches
No Scratches
No Blemishes
No Blemishes
No Color Difference
No Color Difference
Technical Guides

Joint motor housing: aluminum alloy die-casting and CNC post-treatment

For joint motor housings such as robots, collaborative arms and exoskeletons, engineers are most concerned about rigidity, heat dissipation, weight and appearance consistency. Aluminum alloy die casting (Usually ADC12 or A380) Combined with CNC finishing, it is the mainstream path that takes into account both cost and accuracy: die-casting ensures that complex cavities are formed once, CNC post-processing solves coaxiality, flatness and sealing groove tolerances.

Why Joint Motor Housing Preference Aluminum Alloy Die Casting +CNC Combination

The motor casing needs to accommodate the stator, rotor, bearing position, PCB mounting surface, heat dissipation rib or flow channel inside, and the assembly interference and human hand touch should be considered outside. Pure CNC milling aluminum rod (such as 6061-T6) for thin wall and deep cavity machining efficiency is low, tool wear is fast; pure injection molding in thermal conductivity, rigidity and temperature resistance is limited. Aluminum alloy die casting through high temperature molten aluminum under high pressure to fill the mold cavity, can form a complex thin wall (wall thickness can be as low as 1.5 - 2.0 mm) and reinforcing ribs, and then CNC finishing key mating surface, not only control the material waste, but also ensure the stability of key size.

Common material designation and characteristics

  • ADC12: High silicon content, good fluidity, suitable for thin wall and heat dissipation rib structure; moderate strength, density of about 2.74 g/cm³, thermal conductivity of about 96 W/(m·K).
  • A380: The comprehensive mechanical properties are better than ADC12, the tensile strength is about 275 MPa, the yield strength is about 125 MPa, and it is suitable for the casing that bears large assembly preload or vibration load.
  • 6061-T6: If the shell has requirements for corrosion resistance and weldability, it can be processed by CNC machining of profiles or plates, but the cost of deep cavities increases significantly.

Critical Process Parameters and Tolerance Control Boundaries

Die casting process determines the "blank accuracy" of the shell, CNC process determines the "functional accuracy." The division of labor between the two must be clear, otherwise either waste machining allowance, or a key size out of tolerance.

Typical parameters of die casting process

For example, for a 300 - 600 g medium joint shell: melt temperature 650 - 700 ° C, die preheat 150 - 200 ° C, shot speed 20 - 40 m/s for the first stage, 0.5 - 2 m/s for the second stage, and dwell time 100 - 300 ms. These parameters directly affect porosity, porosity and cold shut defect probability. It is recommended that the supplier provide a die-casting Process Specification that includes gate location, vent channel size, and cooling circuit layout.

CNC post-processing tolerance allocation

  • Bearing hole coaxiality: usually ≤0.01 - 0.02 mm, need to complete the processing of both sides of the bearing in one clamping, to avoid the accumulation of secondary positioning errors.
  • PCB mounting surface flatness: ≤0.05 mm, roughness Ra0.8 - 1.6 μm, mirror polishing (Ra0.2 μm) if necessary to prevent electrostatic adsorption dust.
  • Seal groove size: tolerance shall be implemented according to GB/T 1804-m or drawing mark, depth tolerance ±0.05 mm, groove width +0.02/-0 mm, ensure compression ratio of O-ring 15 - 30%.
  • Fin spacing: tolerance ±0.05 mm, avoid interference after assembly caused by heat dissipation channel blockage.

If the casing needs subsequent anodization (Type II, film thickness 8 - 12 μm), 0.05 - 0.10 mm oxidation allowance shall be left after CNC, and the size will increase slightly after oxidation, which shall be considered at the tolerance design stage.

Solution comparison: Die casting +CNC vs pure CNC vs injection molding + metal insert

Comparison of three joint motor housing process routes (based on the elbow joint housing of a medium-sized collaborative robot)
dimensionality ADC12 Die Casting +CNC 6061-T6 Pure CNC PA66+GF30 Injection + Insert
unit weight ~450 g ~480 g ~210 g
heat conductivity coefficient 96 W/(m·K) 150–170 W/(m·K) 0.3–0.5 W/(m·K)
Tolerance capability of critical size ±0.01 mm (after CNC) ±0.005 mm ±0.05 mm
Batch cost (1000 pieces) middle and low tall low
Mold/tooling input High (Die Casting +CNC Fixture) Medium (CNC fixture) High (injection mold + insert positioning)
Delivery time (batch 1000 pieces) 25 - 40 days 30 - 45 days 20 - 35 days
applicable scenarios High rigidity, strict heat dissipation requirements, anodized appearance Ultra-high precision, small batch, no complex thin wall Lightweight, low cost, temperature resistance ≤120 ℃

From the perspective of engineering decision-making: If the chassis performs both structural support and heat dissipation functions, and the batch size is ≥500 pieces, the comprehensive cost of die-casting +CNC is the lowest; if the accuracy requirement is ≤±0.005 mm and the batch size is <200 pieces, pure CNC is more flexible; If the whole machine is extremely sensitive to weight and the working environment temperature is <100 ° C, the injection molding solution is feasible, but it needs to accept the thermal bottleneck and add external aluminum heat sinks.

The Influence of Appearance Quality and Surface Treatment on the Reliability of Cabinet

Joint housings are often exposed to industrial environments. Surface scratches not only affect the appearance, but are more likely to become stress concentration points or corrosion starting points. ShowyMetal emphasizes "high finish, no scratches, batch consistency" in mass production, which relies on three controls:

  • Deburring after die-casting adopts pneumatic purging + nylon roller brush. Direct grinding by grinding machine is prohibited to avoid local overheating deformation.
  • Anodic oxidation adopts Type II sulfuric acid system, film thickness 8 - 12 μm, sealing treatment (hot water sealing at 100 ℃ for 30 min), salt spray resistance test ≥48 h after sealing.
  • Sand blasting + wire drawing combination for matte effect, sand grain size 80 - 120 mesh, wire drawing texture direction consistent with the main stress direction, reduce visual defects.

If the shell needs to be assembled with sheet metal parts or plastic parts, it is recommended to mark the boundary line of surface treatment in the drawing to avoid the fluctuation of preload caused by oxide film covering the thread mating surface.

DFM Recommendations and Common Failure Mode Avoidances

Design End DFM Points

  • Uniformity of wall thickness: avoid local abrupt change>30%, prevent shrinkage porosity and hot joints; make fillet R1.0-R2.0 mm at the root of reinforcing rib.
  • Drawing angle: the side wall of die casting slope 1°-1.5°, blind hole bottom slope ≥3°, easy to demould.
  • Layout of heat dissipation ribs: parallel to the direction of air flow, spacing ≥2.5 mm (considering oxide film thickening) to avoid clogging.
  • Mark surface reservation: If laser engraving is required, reserve a 0.1 mm concave platform to avoid etching through the oxide film.

Typical failures and countermeasures

  • Porosity aggregation: optimize gate position and exhaust groove depth (≥0.5 mm), degas aluminum liquid before die casting (argon stirring for 2 - 3 min).
  • size out of tolerance: measure key size of blank before CNC 100%, establish SPC control chart, isolate abnormal batch immediately.
  • Oxidation color difference: aluminum ingot batch number isolation, anodizing bath solution regular detection (sulfuric acid concentration 150 - 200 g/L, temperature 20 - 30 ℃), the same batch of shell with the same bath treatment.
  • Assembly interference: CNC after three-coordinate sampling (every 50 pieces 1 piece), focus on measuring bearing holes, PCB plane and sealing groove, data provided with the goods.

Acceptance Criteria and Test Means

Before batch shipment, it is recommended to follow the following procedures to ensure traceability of the casing:

  1. Incoming inspection: aluminum ingot furnace number traceability, mechanical properties (tensile/yield/elongation) according to GB/T 1519 sampling.
  2. First article confirmation: CNC first article full size test, coordinate + roughness meter + hardness tester (HV≥35), record reference surface.
  3. Process inspection: sampling 3 pieces of key size every 2 hours, controlling mean and standard deviation.
  4. Full inspection of shipment: inspect appearance (scratch, oxide film uniformity), size, bearing hole concentricity and PCB flatness according to AQL 1.0.
  5. Accompanying documents: material list, CNC program version, coordinate report, oxide film thickness record, salt spray test report (if any).

If the enclosure is used for safety-related parts (such as collaborative robot force-controlled joints), it is recommended to specify key characteristics in the drawings and mark KPC data in the inspection report for the convenience of FMEA and PPAP review by customers.

How long does the joint motor casing die casting +CNC process delivery usually take?

Lot size of 1000 pieces can be delivered in 15 - 25 days (including CNC and surface treatment), and the sampling cycle is about 7 - 10 days. It depends on the drawing complexity, surface treatment type and scheduling load. It is recommended to provide BOM and key size marks when inquiring for quotation for accurate scheduling.

ADC12 or A380, which is better suited for high-vibration joint housings?

If the shell is subjected to high frequency vibration or large assembly preload, A380 is preferred, its tensile strength is about 275 MPa, and its fatigue performance is better than ADC12. ADC12 has better fluidity and is suitable for thin-walled heat dissipation rib structure. The density of the two is similar, and the weight difference can be ignored. It is mainly selected according to mechanical requirements.

How much will the size increase after anodizing? How to reserve tolerances?

Type II anodized film thickness 8 - 12 μm, increase 4 - 6 μm on one side, i.e. increase 8 - 12 μm in diameter direction. 0.05 - 0.10 mm machining allowance shall be reserved here during design, and "size after oxidation" or "size before oxidation" shall be marked on the drawing to avoid acceptance dispute.

How to ensure the appearance consistency of batch cases (no scratches, color differences)?

The key lies in process control: grinding wheel is prohibited for deburring, pneumatic + roller brush is adopted; anodizing is carried out in the same batch and in the same tank, and the sealing water temperature is kept at 100±5 ℃ for 30 min; appearance is sampled according to AQL 1.0 before shipment, and defective batches are isolated for rework. Suppliers can be required to provide salt spray test reports (≥48 h) and film thickness records for each batch as traceability certificates.

Small batch trial production (50 pieces) Can you skip die casting and direct CNC?

Yes. Under the scale of 50 pieces, CNC milling of 6061-T6 or 6082-T6 aluminum bars is more economical (free die-casting mold, mold cost is about 30 - 80,000 yuan). However, attention should be paid to the tool life and cutting thermal deformation of deep cavity machining. It is recommended that the wall thickness is ≥2.5 mm, and the key surface is clamped once. After trial production to verify the accuracy, batch die-casting can significantly reduce the cost.

The process selection of joint motor housing is essentially an engineering trade-off between weight, rigidity, heat dissipation, appearance and cost. Aluminum alloy die casting +CNC combination has clear cost and performance advantages in batch scenarios, but only if the drawings are clearly marked, the tolerance distribution is reasonable, and the surface treatment boundary is clear. If you are developing the next generation of robot joints or exoskeleton actuators, you can send 3D drawings (STEP/IGES) and key size tables to the ShowyMetal technical team. We will provide DFM evaluation, process route suggestions and batch quotations within 24 hours to help you transform your design intentions into mass-produced casings.

Share:
« Previous Medical pacemaker CNC machining titanium shell sealing welding process Next » Robot support: galvanized and passivated carbon steel parts

Related Content

Explore more articles that may interest you.

Send Your Drawing, Get a Quote in 2 Hours.

Send your STEP / DWG / PDF drawing and our engineers reply within 2 hours with a detailed quote including free DFM analysis and process recommendations — no obligation.

Send Drawing for a Quote WhatsApp Us

Send Us Your Drawing — We Handle the Rest

Send your STEP / DWG / PDF drawing and get a detailed quote with free DFM analysis and process recommendations within 2 hours. No minimum order — from 1 piece.

Live inquiries
Michael · GermanyNeed 500 aluminum brackets, please quote
Sophie · FranceLead time for CNC turned stainless shafts?
David · USANeed 1000 injection molded ABS housings
Emma · UKCan you machine 5-axis titanium parts?