CPVC

Chlorinated PVC rated to 93 degree C, for hot water and corrosive fluid systems.

PVC (Polyvinyl Chloride) Grade Details Machinability Verified

Key Specifications

MaterialPVC (Polyvinyl Chloride)
TagCPVC Grade
MOQ100 pcs
Standard Tolerance±0.01 mm
Lead Time15-25 days · Mass Production Rapid Delivery
DFM AnalysisFree
Company
Strength
20 Years of Experience
20 Years of Experience
72 Sets of CNC Machines
72 Sets of CNC Machines
Precision: ±0.01mm
Precision: ±0.01mm
7-15 Days Fast Shipping
7-15 Days Fast Shipping
Quality
Advantages
No Knife Marks
No Knife Marks
No Scratches
No Scratches
No Blemishes
No Blemishes
No Color Difference
No Color Difference

Overview

CPVC Chlorinated Polyvinyl Chloride is a CPVC Grade grade within PVC (Polyvinyl Chloride), widely used in industrial CNC machining due to its balanced mechanical, thermal, and machinability performance.

Chlorinated polyvinyl chloride, heat resistant up to 93°C, suitable for hot water and corrosive fluid systems.

Typical Applications

CPVC Chlorinated Polyvinyl Chloride grades are commonly used in the following fields and scenarios; our CNC machining services can provide custom parts for these industries.

Hot water piping parts
Corrosive fluid valve parts
Chemical pump parts
Fire protection system parts

Key Material Advantages

CPVC Chlorinated Polyvinyl Chloride demonstrates the following core advantages in CNC machining and end-use applications.

Heat resistant up to 93°C
Superior chemical resistance vs PVC
Excellent flame retardancy
Suitable for hot water systems

CNC Machining Guide

The following are key process points when machining PVC (Polyvinyl Chloride) material, to ensure part quality and machining efficiency.

1Tool Selection

Use sharp carbide tools; PVC tends to produce tough burrs during cutting, so maintain sharp edges.

2Temperature Control

PVC has poor thermal stability; it decomposes above 150°C releasing hydrogen chloride, requiring adequate cooling and chip buildup prevention.

3Stress Concentration

PVC is notch-sensitive; internal corners require fillet transitions to prevent cracking during service.

4Cleaning & Protection

PVC surfaces attract dust via static; clean before and after machining and use anti-static packaging to maintain appearance quality.

PVC (Polyvinyl Chloride) - Other Grades

Besides CPVC, PVC (Polyvinyl Chloride) offers several other grades with different characteristics. Click to view details.

Send Us Your Drawing — We Handle the Rest

Send your STEP / DWG / PDF drawing and get a detailed quote with free DFM analysis and process recommendations within 2 hours. No minimum order — from 1 piece.

Live inquiries
Michael · GermanyNeed 500 aluminum brackets, please quote
Sophie · FranceLead time for CNC turned stainless shafts?
David · USANeed 1000 injection molded ABS housings
Emma · UKCan you machine 5-axis titanium parts?