PTFE or solid-lubricant filled wear grade with low friction for oil-free bearings.








Wear-Resistant PPS is a Wear-Resistant Grade grade within PPS (Polyphenylene Sulfide), widely used in industrial CNC machining due to its balanced mechanical, thermal, and machinability performance.
Wear-resistant grade with PTFE or solid lubricant additives, low friction coefficient, suitable for oil-free bearings.
Wear-Resistant PPS grades are commonly used in the following fields and scenarios; our CNC machining services can provide custom parts for these industries.
Wear-Resistant PPS demonstrates the following core advantages in CNC machining and end-use applications.
The following are key process points when machining PPS (Polyphenylene Sulfide) material, to ensure part quality and machining efficiency.
PPS is relatively brittle; use sharp tools with positive rake angles and smaller depths of cut to prevent edge chipping at exit.
Glass-fiber/carbon-fiber-reinforced grades are highly abrasive; use diamond-coated (CVD) or PCD tools.
Air cooling or MQL is recommended; avoid coolant jet impact that can cause localized stress concentration.
Reinforced grades exhibit anisotropy; align machining paths with material flow direction and maintain consistent orientation across batch parts.
Besides Wear Resistant PPS, PPS (Polyphenylene Sulfide) offers several other grades with different characteristics. Click to view details.
Send your STEP / DWG / PDF drawing and get a detailed quote with free DFM analysis and process recommendations within 2 hours. No minimum order — from 1 piece.